tricobalt tetraoxide meaning in Chinese
三氧化三钴
Examples
- The process affect factors of synthesizing the new fine material tricobalt tetraoxide particles were discussed , such as temperature , the solution ph , revolution of stirrer , maturing time , washing water times , drying condition , the color change of process , were discussed , its formation mechanism and structures were systematically studied and discussed , tested the fine particles , the xrd test showed that the peaks became wide
经试验获得均匀凝胶沉淀法新技术优化后的工艺参数为:反应温度控制为273 . 15k左右, ph值为9 . 0 - 9 . 5之间,搅拌转数为300转/分,陈化时间24hr以上,水洗去除杂质,按温度分步烘干。 - It is introduced that the main factor of the lithium - ion battery characteristic of request , indicated the superior electronic properties is mainly related to the cathode material preparation . the paper investigated the synthesis process of tricobalt tetraoxide fine particles by the uniform sol - gel method , using a few analysis equipments test the particles
首先提出均匀凝胶沉淀法新方法,采用此新技术合成了超细co3o4 ,研究了各种因素对合成过程的影响,采用复配沉降剂,获得了絮凝状中间体,经测试证明絮凝状中间体含有大量羟基。